12CRMO4
6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 12CRMO4 →12CrMo4 · EN 10263
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Drawn wire
- Original record status
- Reference transcription of standard
- Standard edition
- BS EN 10263-3:2017
- Table / clause
- Table 3
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
BS EN 10263-3:2017; Heat analysis, mass percent; Values without a stated range are maxima; Notes below the table are retained. No edition is stated on the website; Displayed under this source edition; contract applicability is not established
Verification notes
Standard source: BS EN 10263-3:2017 · Table 3View associated products →12CrMo4 · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Cold-heading wire
- Original record status
- Reference transcription of standard
- Standard edition
- ISO 4954:2018
- Table / clause
- Table B.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018; heat analysis, mass fraction %; values without a stated range are upper limits; see the source page for complete table footnotes. The website does not specify the edition; the source edition is shown here and does not establish contractual applicability.
Verification notes
Standard source: ISO 4954:2018 · Table B.2View associated products →12CrMo4 · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Case-hardening steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ISO 4954:2018
- Table / clause
- Table B.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
ISO 4954:2018, Table B.2 gives heat analysis; A single value is a maximum; a dash is not zero. ; Product-analysis tolerances are listed separately under Table 2/3 of the standard and do not directly widen the heat-analysis composition ranges. ; Optional Al0.020–0.050% to improve cold-heading performance; this is not a universal mandatory minimum. ; Low Si may be agreed in the order, taking hardenability into account; Where hardenability is required, the standard permits limited deviations, except for P/S; C must not exceed 0.01%; see Table 2 for the other requirements.
Verification notes
Original standard Table B.2 and footnotes verified12CrMo4 · EN 10263-3-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10263-3-2017
- Table / clause
- Table 3 and notes 1–3
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Table 3 default; no separate agreement to add Al.
Optional Al 0.020–0.050% selected (Table 3, note 3).
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
Heat analysis mass fraction wt%; Allowable deviations for product analysis shall follow Table 4; this table shall not be expanded unconditionally.. ; Si may be agreed at a lower content or a specific range at the time of ordering; the default in this table is ≤0.30%.. ; To improve cold-heading performance, Al 0.020–0.050% may be optionally added (Note 3); Al is not mandatory for all grades. ; Small deviations for hardenability orders must satisfy Note 2 and Table 4.; P/S shall not be relaxed by this means; the default composition table shall not be automatically expanded.. ; Elements not listed shall not be intentionally added without the purchaser's consent (except additions needed to finish steelmaking); unspecified does not represent zero.. ; This standard is for cold-heading and cold-extrusion, but specific product supply still requires confirmation of dimensions, delivery condition, surface, and performance requirements..
Original condition-branch records
Table 3 default; no separate agreement to add Al.
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Optional Al 0.020–0.050% selected (Table 3, note 3).
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Al | 0.02 ~ 0.05 |
A condition branch must be selected
YesVerification notes
The original English Table 3 and notes have been checked12CrMo4 · DIN EN 10263-3-2002
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10263-3-2002
- Table / clause
- Table 2 and notes a–c
- PDF page references
- 1、8
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
Original DIN EN10263-3 Februar2002 expressly adopts EN10263-3:2001; Composition follows PDF8, Table 2; 2017 is not applied across editions. ; Heat analysis wt%; Si≤.30; a lower content or specified range may be agreed at ordering, but no option is selected without an agreement. ; Note b: hardenability-based orders permit only small deviations, C .01 and the other elements in Table 3; P/S is not applicable; Default limits are not widened; product-analysis tolerances require separate verification. ; Note a: unlisted elements must not be intentionally added except to finish the heat; Residual elements must not impair mechanical properties or end use; unspecified values are not entered as zero. ; The historical table has no general optional Al range under 2017, note 3; the Al option from a later edition is not copied. ; This part covers carburizing steels for cold heading/cold extrusion; dimensions, delivery condition, surface and actual supply still require confirmation.
Verification notes
German source cover, all 25 grades in Table 2 and notes a–c visually checked.12CrMo4 · DIN EN 10263-3-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10263-3:2018-02
- Table / clause
- Tabelle 3, footnote a and note 1–3; Tabelle 4 product-analysis tolerances require separate verification
- PDF page references
- 1、9
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Table 3 default; no separate agreement to add Al.
Optional Al 0.020–0.050% selected (Table 3, note 3).
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
DIN EN 10263-3:2018-02 is the German-language edition of EN 10263-3:2017; Verified according to the heat analysis and notes of Table 3 in the German official version.. ; Table 3 of DIN EN 10263-3:2018-02 specifies the heat analysis mass fraction in wt%.; Allowable deviations for product analysis shall follow Table 4; this table shall not be expanded unconditionally.. ; Si may be agreed at a lower content or a specific range at the time of ordering; the default in this table is ≤0.30%.. ; To improve cold-heading performance, Note 3 of Table 3 allows the optional addition of Al 0.020–0.050%.; This composition variant shall be applied only when explicitly selected.. ; Small deviations for hardenability orders must satisfy Note 2 and Table 4.; P/S shall not be relaxed by this means; the default composition table shall not be automatically expanded.. ; Elements not listed shall not be intentionally added without the purchaser's consent (except additions needed to finish steelmaking); unspecified does not represent zero.. ; This standard is for cold-heading and cold-extrusion, but specific product supply still requires confirmation of dimensions, delivery condition, surface, and performance requirements..
Original condition-branch records
Table 3 default; no separate agreement to add Al.
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Optional Al 0.020–0.050% selected (Table 3, note 3).
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Mn | 0.6 ~ 0.9 |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.25 |
| Si | ≤ 0.3 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Al | 0.02 ~ 0.05 |