12CR13
18 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 12CR13 →12Cr13 · GB /T 1221-2007
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 1221-2007
- Table / clause
- Table 6 · Notes 1/2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Si | ≤ 1 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
Applicability and limitations
Heat analysis, mass fractions wt%; Permissible deviations for product chemical composition shall be separately verified according to GB/T222. ; All values in the table are maximum values except for ranges or minimum values; Values in brackets are the maximum values that may be added or allowed to be contained, and are not required to be added. ; Standard for heat-resistant steel bars; a grade name alone does not establish suitability for cold heading or availability as wire; Processing methods and delivery conditions must be specified in the contract. ; Table 6 Note a marking: Composition grades adjusted relative to GB/T 20878; the ranges listed in this table shall prevail. ; In Table 6, the brackets (0.60) for Ni represent the upper limit that may be added or allowed to be contained.
Verification notes
The original GB/T1221-2007 table and notes have been checked12Cr13 · GB /T 1221-2007
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 1221-2007
- Table / clause
- Table 6 · Notes 1/2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Si | ≤ 1 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
Applicability and limitations
Heat analysis, mass fractions wt%; Permissible deviations for product chemical composition shall be separately verified according to GB/T222. ; All values in the table are maximum values except for ranges or minimum values; Values in brackets are the maximum values that may be added or allowed to be contained, and are not required to be added. ; Standard for heat-resistant steel bars; a grade name alone does not establish suitability for cold heading or availability as wire; Processing methods and delivery conditions must be specified in the contract. ; Table 6 Note a marking: Composition grades adjusted relative to GB/T 20878; the ranges listed in this table shall prevail. ; In Table 6, the brackets (0.60) for Ni represent the upper limit that may be added or allowed to be contained.
Verification notes
The original GB/T1221-2007 table and notes have been checked12Cr13 · GB /T 20878-2007
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless and heat-resistant steels
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 20878—2007
- Table / clause
- Table 4, No. 98
- PDF page references
- 13
- Unit
- Mass fraction (wt%)
- Analysis type
- Standard composition requirements
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
Applicability and limitations
GB/T 20878—2007 tabulated chemical-composition mass fractions wt%; Values in parentheses are maximum permitted additions; conditional expressions require manual interpretation against the original text. Ni ≤0.60 is a maximum permitted addition shown in parentheses. A material-database match does not guarantee cold-heading suitability, actual supply or finished-product strength. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.
Verification notes
GB/T 20878—2007 historical original, Table 4, entry 98. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.12Cr13 · GB /T 1220-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 14975-2012
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 14976-2012
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 20878-2024
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 3280-2015
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 41157.3-2022
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 4238-2015
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | ≤ 0.5 (lower limit not stated) |
| Ni | ≤ 0.75 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 4240-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 4356-2016
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GB /T 8732-2014
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Cu | ≤ 0.3 (lower limit not stated) |
| Mn | ≤ 0.6 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.6 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · GJB 2294A-2014
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 12 ~ 14 |
| Mn | ≤ 0.8 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Si | ≤ 0.8 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · JB /T 6908-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · Q/RP 006-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Mo | ≤ 0.6 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · Q/RP 007-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
12Cr13 · Chinese national standard
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.15 |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.