1116A
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 1116A →1116A · Kobe Steel manufacturer specification (section 6-21)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Free-cutting steel
- Material form
- Reference record
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-21
- PDF page references
- 36
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.13 ~ 0.2 |
| Mn | 1.0 ~ 1.4 |
| P | ≤ 0.07 (lower limit not stated) |
| S | 0.16 ~ 0.23 |
Applicability and limitations
Original composition for free-cutting steel in the Kobe Steel catalogue, section 6-21 (PDF page 36), mass fractions wt%; This is not the original JIS/SAE standard. Actual supply and process applicability require separate confirmation.
Composition conditions
- Original table in section 6-21, mass percent; Dashes and unlisted elements are not entered as zero.
- The 6-21 table lists only C/Mn/P/S; other elements are unspecified and are not entered as zero.
- The KFS series names in parentheses are manufacturer aliases and are not treated as separate grades.