← BackMaterial grade directory

1035 CLASS A

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 1035 CLASS A →

1035 Class A · ASTM A311/A311M-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A311/A311M-2004
Table / clause
Table 1, footnote A; clauses 4.1, 7.1
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV:0.4200–0.5300 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3500–0.4250Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3800–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.32 ~ 0.38
Mn0.6 ~ 0.9
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

Chemical composition is based on ASTM A311/A311M-2004; The reaffirmed 2020 edition remains unavailable. Heat-analysis mass fractions wt%, based on edition 2004, Table 1; Unspecified elements are not entered as zero. Class A is stress-relieved after ordinary-reduction cold drawing; Class B is stress-relieved after greater-reduction cold drawing; Classification does not change the chemical composition in Table 1; mechanical requirements must be checked separately by size and category in Table 2. Table 1, footnote A: 0.15–0.35% is specified only when addition of Pb is required by the order; L is inserted between the second and third characters of the grade designation; Ordinary grades do not automatically include Pb. This standard covers stress-relieved cold-drawn bars; it does not establish cold-heading suitability or an additional supplied product.

Verification notes

Chemical composition follows original 2004, Table 1; The original reaffirmed 2020 edition has not been verified; equivalence between editions is not assumed.

1035 Class A · ASTM A311/A311M-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A311/A311M-2004
Table / clause
Table 1, footnote A; clauses 4.1, 7.1
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV:0.4200–0.5300 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3500–0.4250Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3800–0.4700 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.32 ~ 0.38
Mn0.6 ~ 0.9
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

Heat-analysis mass fractions wt%, based on edition 2004, Table 1; Unspecified elements are not entered as zero. Class A is stress-relieved after ordinary-reduction cold drawing; Class B is stress-relieved after greater-reduction cold drawing; Classification does not change the chemical composition in Table 1; mechanical requirements must be checked separately by size and category in Table 2. Table 1, footnote A: 0.15–0.35% is specified only when addition of Pb is required by the order; L is inserted between the second and third characters of the grade designation; Ordinary grades do not automatically include Pb. This standard covers stress-relieved cold-drawn bars; it does not establish cold-heading suitability or an additional supplied product.

Composition conditions

Verification notes

Table 1 and footnotes in edition 2004 have been checked; equivalence with the 2020 reaffirmed edition is not assumed.
WhatsApp Technical enquiry →