1028B-M
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 1028B-M →1028B-M · Kobe Steel manufacturer specifications (Section 6-13 boron steels)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Boron steels
- Subcategory
- Boron steels
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-13 · carbon boron steel
- PDF page references
- 32
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.23 ~ 0.32 |
| Si | ≤ 0.15 (lower limit not stated) |
| Mn | 0.75 ~ 1.0 |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cr | 0.35 ~ 0.45 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| B | ≥ 0.0008 (upper limit not stated) |
Applicability and limitations
Kobe Steel manufacturer boron steel catalog Section 6-13 (PDF page 32) mass fraction wt% original table; Not the original JIS standard text. Similar JIS grades are for catalog reference only; cold heading and supply shall be confirmed separately.
Composition conditions
- Main elements and table notes in the original Section 6-13: P/S≤0.030%, Cu≤0.25%, B≥0.0008%.; No upper limit given for B; do not guess.
- Similar JIS G3508 grades are for manufacturer catalog reference only, and are not a guarantee of direct equivalence or substitution.