产品中心/ISO 4954
MATERIAL DATA · COLD FORMING
X6CrNiTi18-10 冷镦钢丝
X6CrNiTi18-10 冷镦钢丝技术资料,执行标准为 ISO 4954。查看当前牌号的化学成分、力学性能及相关技术要求。
供货与技术评审 · 睿雄集团受理本产品的供货与技术评审需求;规格、交货状态、数量和检验文件经评审后按订单技术协议确认。
X6CrNiTi18-10 · 冷镦钢丝
01执行标准ISO 4954
02材料牌号X6CrNiTi18-10
03材料形态冷镦钢丝
04交货说明按订单技术条件确认
STANDARD & PROPERTIES
材料技术参数
1.交货条件的组合
表D.1-交货时热处理条件、产品形式和适用要求的组合
| Heat-treat- ment con- dition at delivery | Symbol | Product form a | Steel a | Applicable requirements |
|---|
| Wire rod | Bar | Wire | Ferri- tic | Marten- sitic | Austenit- ic and austenit- ic- ferritic |
| Solution annealed or solution annealed +peeled | +AT or AT+PE | X | X | X | — | — | X | Chemical compo- sition as specified in Table D.2 | Mechani- cal prop- erties as speci- fied in Tables D.3, D.4 and D.6 | Supple- mentary or special re- quirements as specified in Annex Eb |
| Solution annealed +cold drawn | +AT+C | — | X | X | — | — | X |
| Solution an- nealed +cold drawn + solution an- nealed | +AT+C +AT | | X | X | | | X |
| Solution an- nealed +cold drawn+solu- tion annealed + skin passed | +AT+C +AT+ LC | | X | X | | | X |
| Soft annealed or soft annealed + peeled | +A or +A+PE | X | X | X | X | X | — |
| Soft annealed + skin passed | +A+LC | — | X | X | X | X | — |
| Soft annealed + cold drawn + soft annealed | +A+C +A | | X | X | X | X | |
| Soft annealed + cold drawn+ soft annealed + skin passed | +A+C +A+LC | — | X | X | X | X | — |
| Others | Other delivery conditions may be agreed at the time of enquiry and order. |
| a X=applicable,-=not applicable. b If agreed at the time of the enquiry and order |
2.化学组成
表D.2-不锈钢牌号的化学成分 (适用于熔炼分析)
| Designation | % mass fraction a |
|---|
| Steel name | ISO steel number | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu | Others | |
| X6CrNiTi18-10 | 4541-321-00-1 | 0,08 | 1,00 | 2,00 | 0,045 | 0,030 | 17,0 to 19,0 | 9,0 to 12,0 | | — | 1,00 | Ti=5xC to 0,70 |
3.力学性能
表D.6-规定交货条件下马氏体不锈钢的力学性能
化学成分、力学性能、交货状态及其他技术要求应以现行有效标准、客户图纸和订单技术协议为准;网页资料不替代正式质量证明文件。
- 牌号与执行标准
- 线径/截面、交货状态和数量
- 零件图纸、成形工位或失效照片
- 检测项目、证书或报告要求
碳当量计算器 — X6CrNiTi18-10
依据: ISO 4954
化学成分依据: ISO 4954:2018
按所列标准原文转录
产品未注明标准年份;成分采用此处明确列出的已核原文版本。订单适用版本须另行确认,不能推定其他版本相同。
来源原文
Table D.2
当前材料不适用于本页碳钢及低合金钢公式,暂不计算碳当量。
单侧上限表示从 0 到该上限;只有下限时不能确定上界。缺项未知,不按零处理。标准极限组合值不是炉批实测值。
碳当量辅助评估焊接性,不代表冷镦、紧固件强度或焊接工艺获准。上述公式不直接适用于不锈钢、铸铁及有色金属。
方法引用: TWI
碳当量计算器 →
材料参考资料
同牌号参考不代表标准等同、实际供货或替代批准。