04交货说明按订单技术条件确认

材料技术参数

1.交货条件的组合

表C.1交货时热处理条件的组合、产品形式和适用要求

2.化学组成

化学成分来源与适用范围

以下为所列标准版本的参考成分,非炉批实测;订单适用标准、原料与成品要求须分别确认。

来源: ISO 4954:2018 · Table C.2 · C45EC · p.41

元素质量分数 / %
C0.42–0.5
Si≤0.3
Mn0.5–0.8
P≤0.025
S≤0.025
Cu≤0.25

Single values are maxima unless indicated otherwise; unlisted elements and blank cells are not assumed zero. Alternative limits, optional additions and analysis tolerances require the relevant table notes and order agreement. This reference table does not replace the complete standard.

3.力学性能

表C.4-不含硼的非合金钢的力学性能

Steel nameDiameterDelivery condition
+AC or +AC+PE+AR+C+AC+AR+C+AC+LC+AC+C
above mmup to mmRm max. MPaZ min. %Rm max. MPaZ min. %Rm max. MPaZ min. %Rm max. MPaZ min. %
C45EC C45RC25—5906263060——
510600605806262060720—
1040600605806262060710—

4.淬透性要求

表C.7-具有规定 (正常) 淬透性的不含硼的钢种的硬度限值 (H级)

ISO 4954:2022 Table C.7 PDF p.50
Steel nameSym- bolAustenitizing temperature °℃±5℃Limits of rangeHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) ofHardness HRC at a distance from quenched end of test piece(in mm) of
Steel nameSym- bolAustenitizing temperature °℃±5℃Limits of range12345678910111315202530
C45EC+H850max.61605957534739343130292827262524
C45EC+H850min.51463527252423222120——————

使用与订购说明

化学成分、力学性能、交货状态及其他技术要求应以现行有效标准、客户图纸和订单技术协议为准;网页资料不替代正式质量证明文件。

询盘建议提供资料

碳当量计算器 — C45EC

依据: ISO 4954

化学成分依据: ISO 4954:2018

按所列标准原文转录

来源原文

Table C.2

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15已知项贡献,非完整值: 0.5033–0.6500

缺少元素: Cr, Mo, V, Ni

IIW/CEV:碳钢和低合金钢的焊接性初筛。

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B已知项贡献,非完整值: 0.4450–0.5625

缺少元素: Cr, Ni, Mo, V, B

Pcm:主要适用于低碳低合金钢;尤其 C 超过 0.11% 时,须另行确认适用性。

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40已知项贡献,非完整值: 0.4700–0.5925

缺少元素: Mo, Cr, Ni

CET:铁素体钢焊接预热评估,须核对 EN 1011-2 的适用条件。

单侧上限表示从 0 到该上限;只有下限时不能确定上界。缺项未知,不按零处理。标准极限组合值不是炉批实测值。

碳当量辅助评估焊接性,不代表冷镦、紧固件强度或焊接工艺获准。上述公式不直接适用于不锈钢、铸铁及有色金属。